Name
|
Conditioned steel cut wire shot
|
Chemical composition
|
C
|
0.45-0.75%
|
Mn
|
0.60-1.2%
|
Si
|
0.10-0.30%
|
S
|
≤0.05%
|
P
|
≤0.05%
|
Hardness
|
40-52HRC
|
Metallographic structure
|
Deformed pearlite
|
Density
|
≥7.40g/cm3
|
Certifications
Packaging & Shipping
Company Profile
Application
Steel Structural Parts
For the steel structure, the rate of corrosion is mainly
related to the relative humidity of the air as well as the
composition of the pollution in the atmosphere. In order to
prevent or reduce metal corrosion and prolong its service
life, do the surface treatment of steel structures, and
then form a protective film on the metal surface by
painting and spraying to isolate metals from corrosive
media, so that can prevent corrosion of metals.
Hull Segmentation
The quality of hull sandblasting abrasive directly affects
the quality of coating, sandblasting efficiency, kinetic
energy, abrasive consumption and other quality and cost
factors. With the new performance standard for protective
coatings(PSPC),the quality of segmented sand blasting now
has higher requirements. Therefore, the quality of metal
abrasive is particularly important in blasting .
Port Machinery
Port machinery has a high requirement of the corrosion
resistance of steel structure because of the heavy use of
them.Especially the port machinery is often close to some
special circumstances such as humid environment, so the
corrosion is very serious.In this case, requires the use of
sandblasting and coating corresponding to complete
protection of port machinery.
Container
Blast the container after welding can clean up the weld
bead meanwhile make the surface has certain
roughness,increase corrosion resistance of coating. So that
the container can transfer between ships,chassis cars,
trains and rolling stock.